Superalloy barrels

Some time ago, I heard about nickel based superalloys with cobalt based linings being used to make machine gun barrels and tested for some military applications. Today I happened to stumble across this:

http://www.dtic.mil/ndia/2016armament/18355_Armstrong.pdf

I’m sure it would be overkill for a semi auto AR, but I wonder how likely it would be that these would end up on commercially available rifles down the road. While we’re on the subject of superalloys, I also came across a patent from 2012 for John Noveske. It was for an extreme duty machine gun barrel made of H13 tool steel. Pretty tough stuff. This is the same alloy Wilson Combat manufactures their TTU triggers from.

http://www.google.com/patents/US8333029

Thoughts?

Tspeis

Planning on shooting 350 rpm - sustained?

If not, nitriding is adequate and chrome plating is over-kill…

There is an interview out there on the web with John Noveske. These barrels are touched on.

He basically said they were not finically viable. The alloy destroyed tooling. Each barrel had to be sold in the 1000-1500$ range. However they did not last long enough to justify over buying 2-3 of his normal stainless barrels so they never went into full production.

What about gas tubes? Those seem to rupture before the barrel during sustained full auto, right? I wonder how that would hold up paired with a Stellite lined barrel and what the cost would be.

Vseven makes an Inconel one for ~60$

http://www.vsevenweaponsystems.com/collections/upper-parts/products/v7-extreme-environment-gas-tube

Negative, but just because my intended application doesn’t include sustained full auto fire doesn’t mean an alloy more resistant to heat and throat erosion over what’s currently available isn’t desirable. Some of the larger magnum calibers burn through barrels pretty quick and they’re not even gas guns. I understand the price of ammo it would require to burn through a barrel could easily pay for another barrel, but if something better came along at the same price point as current barrels, I’d see no downside to trying it.

I don’t think any H13 barrels were ever sold. Are you sure the interview was about the H13 tool steel barrels and not the 17-4 PH stainless ones? I recall this about the 17-4 PH extreme duty barrels he was doing a while back, but I don’t remember seeing anything about the tool steel though. Not saying it isn’t out there, I just haven’t seen it.

Tspeis

17-4PH is an amazing material. I know John Noveske made a 17-4PH barrel for a M249, however I never heard if any other barrels were made from 17-4PH.

Nickel alloys with cobalt alloy liners? sounds like big $$$ to me. Probably could buy at least 2 CHF barrels and quite a few more regular barrels for the increased cost at a SWAG. If you get more than double the life of a CHF barrel then it might be worth it but that seems like a stretch…

I’m still just waiting for someone to CL a nitrided 41V50 barrel… Seems quite simple enough.

The new Hodge Defense CHF barrels use a proprietary steel and are claiming to be stronger and more accurate than current military barrel offerings, designed to leverage the hard hitting, but high pressure M855A1 ammunition.

interesting. But I fail to understand, why? Anyone can correct me if I am wrong, because I am far from the expert most in here are, but my understanding is the gas tube is meant to be a sacrificial part. It is designed to blow before the barrel does, and is cheap enough to replace without destroying your entire barrel. Using a part like this that is designed to stand up longer to a rigorous firing schedule means it won’t blow, and thus there is a greater chance of your barrel going before this does. Isn’t that counter to what it was originally designed for?

You can do that yourself.

Buy the chrome plated, 41V50 barrel of your choice, and send it out to be nitrided…

There you go.

I was actually thinking of it as someone Nitridring a 41V50 barrel first, and then Chrome Lining it.

Can Chrome be Nitrided? (with no detrimental effects, gain any benefits)

I don’t think so, you’d have to nitride the barrel and then chrome line it as you stated. My understanding is that Chrome will not benefit from feritic nitrocarbuerization.

That would make for one very tough barrel, however I wonder if the benefits would justify the extra cost?

I remember reading that it’s not viable as well when researching barrels in the past, but I do not remember where and therefore until I can find it again I will simply stay under the impression that it shouldn’t be and ask anyone that says otherwise if they can explain why it can be.

That would make for one very tough barrel, however I wonder if the benefits would justify the extra cost?

Should be relatively cheap and easy to execute as well considering how commonplace both barrel finishes are and when compared to super and/or rare alloys/metals.

Found this while researching where I had read about whether chrome itself can be/should be nitrided.

Q.*Is it possible to chrome plate over a nitrided part? —M.M.

A.*Yes, you can chrome plate over a nitrided part. The most critical part of the process is to etch the surface properly prior to plating. Acids should not be used in this process because of the risk of hydrogen embrittlement. Two possible ways of preparing the surface is using sandblasting or tumbling. After plating, the parts should be heat-treated.

http://www.pfonline.com/articles/hard-chrome-on-nitrided-parts

Feritic nitrocarburizing is, by definition, done on steel. Chrome is chrome, not iron so there is no ferrous material to nitrocarburize.

This discussion does make me wonder about the ability to plate chrome alloys onto a bore.

You can chrome plate over a nitrided surface, however, the benefits are not additive in this application. You do not get the added life of a nitrided bore plus the added life of the chrome plated bore, you only get the added life of the chrome plated bore.

Otherwise big really high pressure, hot burning, guns would use this technique to improve barrel life. The M256 120mm tank gun has a chamber pressure in the 85,000 psi range, propellant flame temperatures about 1000 degrees hotter than 5.56mm, and a full charge barrel life of 1500 rounds. If they could get as little as a 10% increase by chrome plating over a nitrided surface, they would do it.

As I posted in the quoted link, the benefit of nitriding a barrel is removed if the nitrided layer of the bore must be removed to allow chrome plating (not uncluding the benefit of the outside of the barrel being nitrided).

My curiosity comes from whether the nitrided layer within the bore must be removed to allow chrome plating to begin with, or if something can be changed in either procedure to allow the to barrel finishes to be applied and have thier effects remain inact to additively applied.

You say that a barrel can be nitrided and then chrome plated, assuming the nitrided layer within the bore remains intact and the chrome plating applied over it, why, exactly, are the effects not cumulative or additive?

Your second pargraph in the post I quoted does not help me understand. I am not trying to be obtuse, but I do admit to having not read up on the subject in some time and being not as interested in the topic as I once was.

And no, I do not subscribe to the line of thinking that just because it’s not being done that way that it means that it’s already been tried, tested and found wanting. I need a bit more than that.