I know most of you have seen Henderson Defenses posts about what guns, optics and mags work. It is pretty telling. I was recently looking at some of his posts on another forum and thought I would grab a couple interesting topics to discuss.
The first one is in regards to the HK MR556:
I purchased a FACTORY brand-new MR556 and it started keyholing after only 10,000 rounds. I was SO pissed because I spent all that money on the gun and it couldn’t last 10,000 rounds. I had barrels from before we even opened the range with 1,000’s of rounds on them from J&T Distributing (chrome-lined) that didn’t keyhole well into the 80,000-100,000 range. I don’t know who makes or made the J&T barrels but I was so pissed that actually wasted the money on a MR556 and that’s all I got from it.
For those that don’t know, the MR556 has a melonited barrel (not Chrome Lined like the 416). From talking to several BIG AR manufacturers, they reported that melonited barrels failed accuracy reqs well under 5,000rds when shot on FA. Apparently on SA, it takes a bit longer to fail (10k). Interesting…
That is really good information. Can you post the name of the article so that we can search for the original? I know we can’t post links to other places but this way we can find it.
Are you sure the HK MR556’s are melonited? I contacted HK to ask about this in 2013 and they told me their MR556 barrels are neither chrome lined nor are they melonited/nitrided. Maybe HK just started meloniting them?
How about other melonited barrels, I have a personal issue with LWRC based off the upper I bout from them, but are their barrels not forged and melonited? What kind reports on these?
As another poster said, it was my impression the MR556 is not melonited or anything similar.
I had seen some stuff in the academic literature about nitrocarburizing breaking down at temperature/pressure extremes but nothing explained in detail. This is the first real world evidence of that i’ve seen. Makes sense when you think about the typical applications being gears, cams and external surface treatments, all things that don’t see 3000+ deg and 40+ksi
That was not surprising regarding the melonite… this was, a little:
USGI mags have outlasted all of the other brands. We use UGSI (Brownell’s with tan follower) and on a mag for mag basis, they have outlasted Pmags and a few of the other mags that we get from mfg’s with new weapons. We don’t have to worry about various generations with different weapons like the MR556, SCAR, F2000, Tavor or a couple of others that use AR15/M4 magazines.
Nothing is this thread is suprising to anyone who has been paying attention and is actually using/building guns.
Melonite is just a way for a manufaturer to claim their barrels have some type of surface treatment while the melonite really does nothing except generate profits on hobby/consumer grade firearms.
Isn’t melonite a treatment and not a coating? And when did HK USA start having the Mr556 barrels melonite? There are companies and people who own MR556 uppers and rifles that have been paying to have their barrel nitrided (see link).
While i cannot find the link, on HKPro forum others have previously addressed the keyholing at 10k round issue and if memory serves me others have had the same problem due to copper fouling that was fixed after a thorough cleaning of the barrel (due to being non chrome lined or melonited).
Right. With talking with some of these companies, it is pretty well assumed that the pressure and heat is what kills the barrels. Since that MR556 was shot SA, it just took longer.
On the flip side, quality CL barrels don’t key hole till 20k or longer.
I guess copper fouling could do it, you would have had to completely ignore cleaning your barrel for YEARS. To date in all my years, I have never seen this. Copper fouling wasn’t the case for the Vegas range. They clean and lube their guns regularly.